This jar is glazed with my G3948A cone 6 iron red recipe. It employs two Ferro Frits: High soda, low boron, low alumina 3110 and high boron, high soda/calcia, low alumina 3134. These frits are becoming increasingly expensive and difficult to get in many parts of the world (even North America).
A potter in the UK has access to locally produced BPS (Bath Potters' Supplies) frits. They have ones that roughly match the Ferro products, calling them "Standard Borax" and "High Alkaline". These frits are shown side-by-side in this screenshot; they are too different to just substitute; chemistry is essential here. My original G3948A recipe is also shown side-by-side with the chemical equivalent I just calculated. I am using generic talc, kaolin and spodumene materials (the chemistry of these needs to be entered to make the calculation more accurate, especially the spodumene, an important factor in how this glaze fires).
I will update this post as we get more information and, finally, fired tests. Hopefully we can bring floating blue to the UK using this same method.

This picture has its own page with more detail, click here to see it.
This spoon jar is glazed with the G3948A recipe. It was fired using our standard cone 6 C6DHSC slow cool schedule. The body is Plainsman Coffee Clay. The inside glaze is GA6-B, although honey transparent, it fires jet black on this body. The metallic outer appearance was achieved because of the thick application. But this glaze has a fluid melt and should have run on to the kiln shelf. Why didn't it do that? Because of the way I glazed it. The inside was done first. Then wax was applied over the rim and down the inside for a couple inches. Then I applied a thin layer of the iron red to the bottom half to act as a catch glaze (by pushing the piece down into the bucket of dipping glaze for only a second). That dried in about 5 seconds, enabling flipping it over and pressing it down to do the upper half. I held it down longer and got a much thicker layer (with a little overlap with the thin section). During firing it all evened out - leaving only a little evidence of this method near the base.

This picture has its own page with more detail, click here to see it.
Amaco Ancient Copper, is on the left. Right is G3948A, our iron red (a publicly available recipe). Both of these have been fired using the C6DHSC slow cool firing schedule. As you can see, the PC-56 crystallizes more, matting the surface in the process. But if cooled normally (e.g. using the PLC6DS schedule) it does fire similar to G3948A. Likewise, G3948A can be made to crystallize more if the iron oxide percentage is increased in the recipe (I use black iron, it is a little less concentrated than red but does not gel the slurry). The recipe offers excellent slurry properties when mixed as a dipping glaze. Our version uses Spodumene (which has 7% Li2O). Of course, lithium materials are very expensive these days, but that is what is needed for this effect. If you make a brushing glaze of it using my instructions, only about 70g of spodumene is needed to make a 500ml jar. At current material costs, I could make 3 jars for $10 worth of powdered materials!

This picture has its own page with more detail, click here to see it.
This is G3948A (similar to the popular Amaco Ancient Copper product). To get this stunning result, it needs to be applied thickly. Therefore, it runs a lot. But the catcher glaze around the bottom of these mugs has stopped the flow. The catcher is a glossy black, G3914A (but Amaco Obsidian would also likely work). I have learned to put it on with the right height (about 2cm) and right thickness, and then apply wax emulsion to prevent the iron red glaze from sticking during dipping. The inside glaze, G2926B, is one I have tested and developed to fit Plainsman clay bodies as a liner.
| Glossary |
Iron Red Glaze
A type of ceramic glaze, typically fired around 2200F, where iron oxide in the cooling glass precipitates out to form a striking red crystalline mesh on the surface. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
Buy me a coffee and we can talk