This is the Testdata Editor window. As soon as I save the entry, it will calculate the porosity (more precisely, the water absorption) and show it in the ABS column (with the red title) for specimen 7.
| Glossary |
Digitalfire Insight-Live
A cloud-hosted ceramics-targeted LIMS (lab info management system). It does glaze chemistry and physical testing the “Digitalfire way”. For technicians, educators, potters and hobbyists. |
| Glossary |
Clay Body Porosity
In ceramics, porosity is considered an indication of density and therefore strength and durability. Porosity is measured by water absorption, the weight increase when boiled in water. |