This unbelievable body is made from dolomite, 65% of it. There is 35% ball clay to give it workability and 5% Ferro frit 3110. The frit stabilizes it so that the fired body does not rehydrate. This has a porosity of 35%! And that porosity is stable across the entire range we have fired it at (cone 06-6). The single-layer on the lower portion has been completely absorbed, the double-layer on the upper is almost gone.
| Glossary |
Clay Body Porosity
In ceramics, porosity is considered an indication of density and therefore strength and durability. Porosity is measured by water absorption, the weight increase when boiled in water. |
| Materials |
Dolomite
An inexpensive source of MgO and CaO for ceramic glazes, also a highly refractory material when fired in the absence of reactant fluxes. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
Buy me a coffee and we can talk