These are Plainsman PR3B and PR3D. The 3B bars are fired from cone 8 down to 2 (top to bottom) and the 3D ones from cone 9 down to 3. The 3B has added Nepheline to achieve zero porosity below cone 4 (to make an even better MNP). When plus 325 mesh particles are removed from the 3D is becomes quite plastic, suitable as a stoneware by itself (which we call MNS). And it reaches zero porosity around cone 6. 3D is lighter burning and cleaner, 3B is more vitreous and plastic.

This picture has its own page with more detail, click here to see it.
The clay is Plainsman 3B.
Left: Without processing, other than grinding to 42 mesh (currently the finest Plainsman can grind on a practical scale). When fired toward zero porosity (water absorption) it burns like this (at cone 6, 8, 9, 10 and 10R bottom to top). Of course, these are not big issues for non-vitreous rustic bodies fired at cone 6. The speckle and bloating are caused by impurity iron-bearing particles and others having an LOI (they decompose and produce gases that cause the bloats).
Right: The impurity particles make up a small percentage; they can be removed in the lab by sieving to produce a natural porcelain that fully vitrifies by cone 6 (the middle bar). Only about 5% of the material was removed to produce this amazing product (I call it MNP).
Imagine what could be done if this raw material could be mined further east, where clay quality is much better!
| Projects | Plainsman 3D, Mother Nature's Porcelain/Stoneware |
| Materials |
3D Clay
Fine particled, clean, silty stoneware clay containing natural feldspar |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
Buy me a coffee and we can talk