Left: Traditional blue material, could be 20 years old.
Center: A shipment we got in Feb 2014.
Right: A shipment in Oct 2014.
Front: 10 gram balls prepared for a melt-flow GBFL test.
The blue powder is the most difficult to form (therefore the least plastic) after water has been added, the tan one is the easiest.
| Materials |
Cornwall Stone
Cornwall stone was a low-iron feldspar material used primarily as a flux in clay bodies and glazes |