Consider how valuable your glaze and body development records are. Are they in a three-ring binder? Or do you have pictures and notes scattered across apps on your phone? If you're testing, adjusting, or developing glazes, bodies, underglazes or engobes, traditional notebooks and binders are holding you back. They don't have keywords, and they are only grouped, not categorized. With Insight-live, you can link recipes to each other and to important details like photos, materials, firing schedules and URLs. Organize test recipes into projects, classify them with typecodes (tokens), calculate chemistry, and create mix tickets. Research materials and perform keyword searches. Put anything side-by-side to study and determine the next move. Physical notebooks can’t do this—but your account at Insight-live.com can!

This picture has its own page with more detail, click here to see it.
If you do DIY pottery glazing you may have recipes scribbled onto cards like this. But the card is not the big issue here; it is that recipe! It really needs some work. Here is what could be done.
-Add this as a recipe in an account at insight-live.com (and assign it a code number to write on all test specimens) to start a testing project. Along the way document it with pictures, firing schedules, general notes, etc.
-With all that feldspar, it is sure to craze, reducing the high thermal expansion K2O it contributes in favor of low expansion MgO (from talc) is the first fix to try.
-With all that clay (29 total) it is likely to crack while drying (and then crawl during firing). Try reducing shrinkage with 29 kaolin (no ball clay). If it still cracks, substitute some for calcined kaolin.
-And those colorants: It is better to use cobalt oxide than carbonate. A burnt umber increase could be tested to eliminate the need for both the manganese and iron (since it supplies both and has zero LOI). Better yet, remove all four and use a black stain (7% would likely be enough).
-Perhaps the best option is to get a different glaze recipe. This is a calcium matte to G1214Z1 would be a good start. For a more pleasant surface, G2934.

This picture has its own page with more detail, click here to see it.
This two-inch stack of clay body and glaze mix tickets represents only about half of my testing over the past year. Along the way, I also added thousands of photos to my Insight-live.com account. Looking at this pile, I realized why I am testing more: Organized records make it easier to keep multiple projects moving. I can see what I have tried, compare results and pick up where I left off. Each test builds on earlier work, and that visible progress motivates me to keep going. If you want to do DIY glazes and bodies, this is the secret is good record-keeping.

This picture has its own page with more detail, click here to see it.
A promising test is frustratingly difficult to repeat if you cannot identify how you made it. A code number on each specimen links it to its recipe, firing schedule, pictures and notes—and to earlier and later versions in the same project. These mugs and the test bar are made from the same experimental material (called “Battle Clay”). Their code connects them to the records for that test mix. Pretty much everything I have ever made has been a test, and thus has code numbers on the bottoms. I can pick up a 40-year old specimen and find its history, or open the record and locate the matching pieces (in my Insight-live.com account).
| URLs |
https://digitalfire.com/university/insight-live/overview/Insight-Live%20Overview.html
Insight-Live.com Overview Video |
| Glossary |
Code Numbering
In a ceramics lab, studio or classroom specimens of hundreds of glazes and bodies may be present. A code numbering system that links these to written or computer records is essential. |
| Glossary |
Digitalfire Insight-Live
A cloud-hosted ceramics-targeted LIMS (lab info management system). It does glaze chemistry and physical testing the “Digitalfire way”. For technicians, educators, potters and hobbyists. |
| Glossary |
Glaze Recipes
Stop! Think! Do not get addicted to the trafficking in online glaze recipes. Learn to make your own or adjust/adapt/fix what you find online. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
Buy me a coffee and we can talk