This is the G2934Y matte base with overglaze decoration fired at cone 6. Although this matte has a high melt fluidity, overglaze decoration can be successful as long as it is not applied too thick and not overfired. But in this case the glaze is thickly applied. Once the critical thickness boundary is passed, the glaze's ability to hold overglaze in place quick degrades. The G2934 recipe has less melt fluidity and fires to the same surface, it would would be a better choice as the base glaze in this case (and could be applied thicker). However this Y variation would be a good choice as the medium if you want to make your own overglaze brushable colors.
| Troubles |
Bleeding Colors
In ceramics, the edges of overglaze and underglaze color decoration often bleeds into the over or under glaze. How can this be avoided. |
| Recipes |
G2934Y - Cone 6 Magnesia Matte Low LOI Version
The same chemistry as the widely used G2934 but the MgO is sourced from a frit and talc instead of dolomite. It has a finer surface, less cutlery marking and staining. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
Buy me a coffee and we can talk