Our theoretical chemistry is fairly close to this (notice these numbers are not precise, they indicate a range or minimum).
| Materials |
Spodumene
Spodumene is a lithium sourcing feldspar, an alternative to lithium carbonate to supply Li2O to ceramic glazes. Contains up to about 8% Li2O. |