These were fired at cone 04 using Spectrum glazes. Both were glazed using the same brushing technique. The one on the left has 4 coats, on the right three coats. The high spots on the throwing rings and the edges of contours are more visible when the glaze is thinner.
| Glossary |
Brushing Glaze
Hobbyists and increasing numbers of potters use commercial paint-on glazes. It's convenient, there are lots of visual effects. There are also issues compared to dipping glazes. You can also make your own. |