This is a 50:50 mix of calcine and raw Alberta Slip plus 5 parts Mason 6600 black stain, 5 Mason 6666 black and 7 iron.
| Recipes |
GA10-D - Alberta Slip Black Cone 10R
You can make a black glaze at cone 10R using only 1% black stain in a 100% calcine:raw mix of Alberta Slip |
| Glossary |
Metallic Glazes
Non-functional ceramic glazes having very high percentages of metallic oxides/carbonates (manganese, copper, cobalt, chrome). |
| Materials |
Alberta Slip
Albany Slip successor - a plastic clay that melts to dark brown glossy at cone 10R, with a frit addition it can also host a wide range of glazes at cone 6. |