Double-layered on top half. Fired with the PLC6DS schedule.

This picture has its own page with more detail, click here to see it.
This melt fluidity tester demonstrates that the cone 6 G1214Z recipe fires highly melt fluid, much more than one might expect from a matte glaze. When applied as a thin layer on pottery it does behave as a matte glaze. A quick look at its oxide chemistry reveals the reason: High CaO and a low Si:Al ratio. Unfortunately, many matte glazes are such simply because they are not melted enough. Others have to much SiO2 and require very slow cooling in the kiln to achieve results.
| Recipes |
G1214Z1 - Cone 6 Silky CaO matte base glaze
This glaze was born as a demonstration of how to use chemistry to convert a glossy cone 6 glaze into a matte. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
Buy me a coffee and we can talk