This is G3948A iron red glaze fired using the C6DHSC schedule. The casting body is L4768D, a fast-casting mix made using OptiKast kaolin, nepheline syenite, silica and raw umber. It fires almost black and is highly vitreous and strong. The inside glaze is the GA6-B base Alberta Slip super gloss functional. These are part of a project where we are documenting step-by-step how to make the mold and casting slip.

This picture has its own page with more detail, click here to see it.
The center bottle is a standard glass one, the other two are ceramic, cast out of my version 1 plaster mold. The stopper fits perfectly. The clay is Plainsman M370 + 10% raw umber, it fires black. The glaze is GA6-B, an amber transparent that produces a deep glass-like effect over the dark burning body. They were fired using the C6DHSC firing schedule. These bottles are a testament to how 3D printing and 3D design now make it possible for even casual potters to make pieces never before practical or even possible.
Buy me a coffee and we can talk