Clays of very high plasticity often stiffen during storage in the bag. This is Plainsman Polar Ice, it contains 4% VeeGum. This slug is like a brick, yet it will loosen up completely. But it is far too stiff to attempt wedging. However, simply throwing it on the floor a few times (turning it each time) will pre-soften it enough to be able to wedge. Then, before you know it, it is too soft and needs to be put on a plaster table to stiffen it before throwing.
| Media |
A 3-minute Mug with Plainsman Polar Ice
Tony Hansen takes you through the steps from opening the box and wedging the clay to taking the fired mug from the kiln. |
| Glossary |
Clay Stiffness
In ceramics, clays exhibit plasticity in accordance with their recipe but also the water content. The stiffness considered correct varies for different types of forming methods. |
| Glossary |
Wedging
The process of mixing a plastic clay by hand before forming it. Similar to kneading of bread dough, it is considered an essential step by most potters. |