This occurs as they cool in the kiln. The slower the cooling and the more iron oxide there is, the bigger and more plentiful these crystals will be.
| Glossary |
Tenmoku
Tenmoku is a kind of high temperature reduction firing ceramic glaze. Glossy, very dark brown or maroon, fluxed by iron oxide to have high melt fluidity. |