Wet location sealed switch used on mixer. The electrical-in is sealed using silicone.

This picture has its own page with more detail, click here to see it.
This is a heavy-duty one-speed mixer, homemade, with a 1/3 hp motor. It can handle up to ten gallons of high-density glaze or body slurry.
| Articles |
A One-speed Lab or Studio Slurry Mixer
A single-speed lab mixer can be made for much less money than buying a commercial unit. Using it you can slurry up a 100 lb batch of porcelain powder in minutes and it will be smooth as silk. |