Sanitary ware factories optimize their slips to have the lowest possible specific gravity for production volume reasons. Potters would be happy with 1.7 SG whereas numbers approaching 1.9 SG are common in factories. They often teeter on the edge of issues like this (sections softening causing localize warping) and inexperienced technicians can be unaware of the critical balances needed to prevent loss in production.
| Glossary |
Deflocculation
Deflocculation is the magic behind the ceramic casting process, it enables slurries having impossibly low water contents and ware having amazingly low drying shrinkage |
| Glossary |
Sanitary ware
A type of porcelain zircon-glazed ceramic that includes bathtubs, sinks, toilets, etc. |
| Troubles |
Casting Slip Problems
Casting slips are deflocculated in order to reduce water content. It is important to understand this phenomenon and know how to assess a slurry to know what it needs. |