Plainsman Fire-Red fireclay fired to cone 10R. This shows the effect of reduction where the body is exposed to the kiln atmosphere (very dark burning) and where it is not (inner foot ring).
| Glossary |
Reduction Firing
A method of firing stoneware where the kiln air intakes and burners are set to restrict or eliminate oxygen in the kiln such that metallic oxides convert to their reduced metallic state. |
| Materials |
Fireclay
|