Body is Plainsman P580. Far left: G2894 Ravenscrag Tenmoku with 10% whiting and 10% iron oxide added. Center: Pure Alberta Slip plus 5% whiting and 1% iron oxide. Right: Pure Alberta Slip plus 5% whiting and and 2% iron. The Alberta Slip versions are less messy to use because so much less iron is needed (iron also causes the slurry to gel). The Ravenscrag and higher iron Alberta Slip versions are running, they are too fluid. The rust colored crystals are not developing the way they did with these glazes on an iron stoneware (in the same firing).

This picture has its own page with more detail, click here to see it.
All of these are on a cone 10 reduction fired iron stoneware (Plainsman H443). Far left: G2894 Ravenscrag Tenmoku with 10% whiting and 10% iron oxide added. Center: Pure Alberta Slip plus 5% whiting and 1% iron oxide. Right: Pure Alberta Slip plus 5% whiting and and 2% iron. The Alberta Slip versions are less messy to use because so much less iron is needed (iron also causes the slurry to gel). The Ravenscrag version is running, it is too fluid. Likely 5% calcium carbonate would be enough (and maybe less iron).
| Recipes |
GA10-B - Alberta Slip Tenmoku Cone 10R
You can make a tenmoku from Alberta Slip by adding only 2% iron oxide and 5% calcium carbonate |
| Glossary |
Tenmoku
Tenmoku is a kind of high temperature reduction firing ceramic glaze. Glossy, very dark brown or maroon, fluxed by iron oxide to have high melt fluidity. |