| Monthly Tech-Tip | No tracking! No ads! | |
Frits are made by melting mixes of raw materials in a special furnace, then pouring the molten mix into water. That produces these shards of glass. These are ground to the white powder we use to make glazes.
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |