Made by Dawn Candy. Clay is Plainsman M370. Fired at cone 6.
| Glossary |
Slip Trailing
A technique used by potters to decorate ware. Neutral and colored slips, clay in thick paste form, are trailed onto the ware (in raised lines and strokes) to create tactile designs. |