This is Plainsman translucent Polar Ice firing at cone 6 with a transparent base glaze. Made by Tony Hansen in 2014.
Recipes |
G2926B - Cone 6 Whiteware/Porcelain Transparent Base Glaze
A base transparent glaze recipe created by Tony Hansen for Plainsman Clays, it fires high gloss and ultra clear with low melt mobility. |
---|---|
Glossary |
Base Glaze