Serial Number: AJ24133
Run/Test Number: L4062A
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G1947U
Glaze Outside - G2571A
Engobe - L3954N
Clay Body - H550
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 100 mm (3.9 in)
Depth at rim (including handle) - 132 mm (5.2 in)
Height - 108 mm (4.3 in)
Weight - 376 grams (13.3 oz)
Price:$35.00 (Not for sale, pieces being held for demo purposes)