Serial Number: AJ24335
Run/Test Number: P6747
Technique: Thrown, incised, dip-glazed
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G1947U
Glaze Outside - G1947U
Clay Body - P700
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 90 mm (3.5 in)
Depth at rim (including handle) - 123 mm (4.8 in)
Height - 106 mm (4.2 in)
Weight - 321 grams (11.3 oz)