Zero3 fritware porcelain hash-tag mug

Serial Number: AJ24161
Run/Test Number: L3924C
Technique: Thrown, leather-hard under-glaze decorated, incised, 1650F bisque fired, dip-glazed

Firing Schedule - C04PLTP
Temperature - Cone 03
Glaze Inside - G2931K
Glaze Outside - G2931K
Clay Body - L3924C
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 88 mm (3.5 in)
Depth at rim (including handle) - 120 mm (4.7 in)
Height - 129 mm (5.1 in)
Weight - 293 grams (10.3 oz)

Price:$35.00 (Not for sale, pieces being held for demo purposes)