Black matte mug

Serial Number: AJ24431
Run/Test Number: P7027
Technique: Thrown, liner-glazed inside, dip-glazed outside

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926BL
Glaze Outside - G2934Y Black
Engobe - L3954B
Clay Body - M370
Foot Style - Unglazed flat black engobed
Width at rim (perpendicular to handle) - 89 mm (3.5 in)
Depth at rim (including handle) - 127 mm (5.0 in)
Height - 111 mm (4.4 in)
Weight - 372 grams (13.1 oz)