Gunmetal black stoneware mug

Serial Number: AJ24146
Run/Test Number: L3789C
Technique: Mug and handle slip cast, jigger-finished, liner-glazed inside, dip-glazed outside

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2934Y Black
Clay Body - L3798G
Foot Style - Foot ring
Width at rim (perpendicular to handle) - 93 mm (3.7 in)
Depth at rim (including handle) - 122 mm (4.8 in)
Height - 110 mm (4.3 in)
Weight - 440 grams (15.5 oz)