Red matte reduction glazed mug

Serial Number: AJ50022
Run/Test Number: L4686C
Description: Fired at cone 6 oxidation on buff stoneware. By Tony Hansen.

Temperature - Cone 10R
Glaze Inside - GR10-C
Glaze Outside - G2571D Red
Clay Body - H570
Foot Style - Flat unglazed
Width at rim (perpendicular to handle) - 91 mm (3.6 in)
Depth at rim (including handle) - 122 mm (4.8 in)
Height - 102 mm (4.0 in)
Weight - 313 grams (11.0 oz)