Serial Number: AJ24435
Run/Test Number: P6954
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G3914A
Glaze Outside - G2934Y Black
Clay Body - M340
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 100 mm (3.9 in)
Depth at rim (including handle) - 132 mm (5.2 in)
Height - 122 mm (4.8 in)
Weight - 362 grams (12.8 oz)
Price:$40.00 (Not for sale, pieces being held for demo purposes)