Serial Number: AJ24127
Run/Test Number: P6722
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - GA6-B
Glaze Outside - GR6-M
Clay Body - M390
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 100 mm (3.9 in)
Depth at rim (including handle) - 132 mm (5.2 in)
Height - 126 mm (5.0 in)
Weight - 403 grams (14.2 oz)
Price:$45.00 (Not for sale, pieces being held for demo purposes)