Serial Number: AJ24104
Run/Test Number: P6768
Technique: Thrown, incised, dip-glazed
Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - GR6-M
Glaze Outside - GR6-M
Clay Body - M332
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 102 mm (4.0 in)
Depth at rim (including handle) - 133 mm (5.2 in)
Height - 124 mm (4.9 in)
Weight - 469 grams (16.5 oz)
Price:$35.00 (Not for sale, pieces being held for demo purposes)