Serial Number: AJ50017
Run/Test Number: L4484K1
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table.
Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - GA6-B
Glaze Outside - G3939E
Clay Body - L4484K1
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 95 mm (3.7 in)
Depth at rim (including handle) - 129 mm (5.1 in)
Height - 95 mm (3.7 in)
Weight - 344 grams (12.1 oz)