Dark honey-glazed MNP porcelain mug

Serial Number: AJ24073
Run/Test Number: L4283
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table.

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - GA6-B
Clay Body - L4283 MNP
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 87 mm (3.4 in)
Depth at rim (including handle) - 120 mm (4.7 in)
Height - 90 mm (3.5 in)
Weight - 271 grams (9.6 oz)

Price:$55.00 (Not for sale, pieces being held for demo purposes)


PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy