Serial Number: AJ24150
Technique: Hand-assembled, pour-glazed inside, waxed, liner-glazed inside, dip-glazed outside
Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2934Y Yellow
Clay Body - M370
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 93 mm (3.7 in)
Depth at rim (including handle) - 120 mm (4.7 in)
Height - 100 mm (3.9 in)
Weight - 331 grams (11.7 oz)
Price:$25.00 (Not for sale, pieces being held for demo purposes)