Serial Number: AJ24149
Run/Test Number: L4062A
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G2571A
Glaze Outside - G2571A
Engobe - L3954N
Clay Body - B-Mix
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 105 mm (4.1 in)
Depth at rim (including handle) - 136 mm (5.4 in)
Height - 91 mm (3.6 in)
Weight - 382 grams (13.5 oz)
Price:$30.00 (Not for sale, pieces being held for demo purposes)