Serial Number: AJ24074
Run/Test Number: L4283
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table.
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - GA6-B
Clay Body - L4283 MNP
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 88 mm (3.5 in)
Depth at rim (including handle) - 117 mm (4.6 in)
Height - 100 mm (3.9 in)
Weight - 313 grams (11.0 oz)