Serial Number: AJ24400
Run/Test Number: P6699
Technique: Hand-rolled and assembled, engobed inside and top outside, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G1947U
Glaze Outside - G2571A Bamboo
Engobe - L3954N
Clay Body - P600
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 97 mm (3.8 in)
Depth at rim (including handle) - 128 mm (5.0 in)
Height - 101 mm (4.0 in)
Weight - 322 grams (11.3 oz)
Price:$40.00 (Not for sale, pieces being held for demo purposes)