Digitalfire is facing a takedown order from Plainsman Clays. They are revoking permission to "use any Plainsman content" "on any platform". This is broad and vague enough, and this site large enough, that I am unable to comply or even interpret it in the short timeframe (June 27). Insight-live.com general operation is not affected by this.

Porcelain reduction-fired mug

Serial Number: AJ24090
Run/Test Number: P6572
Technique: Thrown, incised, dip-glazed

Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G1947U
Glaze Outside - G1947U
Clay Body - P700
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 90 mm (3.5 in)
Depth at rim (including handle) - 117 mm (4.6 in)
Height - 111 mm (4.4 in)
Weight - 306 grams (10.8 oz)

Price:$35.00 (Not for sale, pieces being held for demo purposes)


PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy