Bamboo tan incised stoneware mug

Serial Number: AJ24411
Run/Test Number: L4040A
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - GR10-C
Glaze Outside - G2571A Bamboo
Engobe - L3954N
Clay Body - H555
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 99 mm (3.9 in)
Depth at rim (including handle) - 129 mm (5.1 in)
Height - 104 mm (4.1 in)
Weight - 357 grams (12.6 oz)

Price:$40.00 (Not for sale, pieces being held for demo purposes)