Bamboo tan incised stoneware mug

Serial Number: AJ50031
Run/Test Number: L4168G8
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G1947U
Glaze Outside - G2571A
Clay Body - H440
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 95 mm (3.7 in)
Depth at rim (including handle) - 133 mm (5.2 in)
Height - 95 mm (3.7 in)
Weight - 353 grams (12.4 oz)