Red and black Polar Ice porcelain mug

Serial Number: AJ24427
Run/Test Number: P7027
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G3914A
Glaze Outside - G2934Y Red
Clay Body - M370
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 93 mm (3.7 in)
Depth at rim (including handle) - 122 mm (4.8 in)
Height - 113 mm (4.4 in)
Weight - 356 grams (12.5 oz)