Serial Number: AJ24317
Run/Test Number: P6928
Technique: Thrown, incised, dip-glazed
Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G3914A
Glaze Outside - G2934Y Black
Clay Body - M370
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 99 mm (3.9 in)
Depth at rim (including handle) - 132 mm (5.2 in)
Height - 120 mm (4.7 in)
Weight - 378 grams (13.3 oz)
Price:$40.00 (Not for sale, pieces being held for demo purposes)