Black MNS stoneware mug

Serial Number: AJ24405
Run/Test Number: L4492
Technique: Thrown, incised, dip-glazed

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G3914A
Glaze Outside - G2934
Clay Body - L4492 MNS
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 94 mm (3.7 in)
Depth at rim (including handle) - 125 mm (4.9 in)
Height - 105 mm (4.1 in)
Weight - 310 grams (10.9 oz)

Price:$35.00 (Not for sale, pieces being held for demo purposes)