Floating-blue stoneware mug

Serial Number: AJ24394
Run/Test Number: L4471C
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - C6DHSC
Temperature - Cone 5
Glaze Inside - GR6-M
Glaze Outside - GR6-M
Clay Body - M390
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 96 mm (3.8 in)
Depth at rim (including handle) - 125 mm (4.9 in)
Height - 120 mm (4.7 in)
Weight - 333 grams (11.7 oz)

Price:$40.00 (Not for sale, pieces being held for demo purposes)