Serial Number: AJ240160
Run/Test Number: L4249A
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table.
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - GA6-A
Glaze Outside - GA6-C
Clay Body - L4249A MNS
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 100 mm (3.9 in)
Depth at rim (including handle) - 127 mm (5.0 in)
Height - 124 mm (4.9 in)
Weight - 425 grams (15.0 oz)