Serial Number: AJ240150
Run/Test Number: L4208C
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2826B
Glaze Outside - GA6-B
Clay Body - L4208C MNS
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 96 mm (3.8 in)
Depth at rim (including handle) - 125 mm (4.9 in)
Height - 103 mm (4.1 in)
Weight - 378 grams (13.3 oz)
Price:$45.00 (Not for sale, pieces being held for demo purposes)