Floating-blue stoneware mug

Serial Number: AJ24363
Run/Test Number: L4471G
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - GA6-B
Glaze Outside - GR6-M
Clay Body - M390 test
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 95 mm (3.7 in)
Depth at rim (including handle) - 130 mm (5.1 in)
Height - 123 mm (4.8 in)
Weight - 369 grams (13.0 oz)

Price:$35.00 (Not for sale, pieces being held for demo purposes)