Oatmeal glazed mug

Serial Number: AJ50013
Run/Test Number: L4449J
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G3914A
Glaze Outside - G3933E
Clay Body - Coffee Clay
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 98 mm (3.9 in)
Depth at rim (including handle) - 132 mm (5.2 in)
Height - 123 mm (4.8 in)
Weight - 418 grams (14.7 oz)