Matte red mug

Serial Number: AJ24380
Run/Test Number: P6973
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G3914A
Glaze Outside - G2934Y Red
Clay Body - M370
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 104 mm (4.1 in)
Depth at rim (including handle) - 136 mm (5.4 in)
Height - 132 mm (5.2 in)
Weight - 386 grams (13.6 oz)

Price:$50.00 (Not for sale, pieces being held for demo purposes)


PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.