Bamboo tan incised stoneware mug

Serial Number: AJ24396
Run/Test Number: P6679
Technique: Hand-rolled and assembled, engobed inside and top outside, incised, dip-glazed

Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G2571A Bamboo
Glaze Outside - G2571A Bamboo
Engobe - L3954N
Clay Body - H550
Foot Style - Unglazed flat
Width at rim (perpendicular to handle) - 97 mm (3.8 in)
Depth at rim (including handle) - 132 mm (5.2 in)
Height - 107 mm (4.2 in)
Weight - 306 grams (10.8 oz)

Price:$40.00 (Not for sale, pieces being held for demo purposes)