Bamboo tan incised stoneware mug

Serial Number: AJ24327
Run/Test Number: P6902
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed

Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G2571A Bamboo
Glaze Outside - G2571A bamboo matte
Engobe - L3954N
Clay Body - H450
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 112 mm (4.4 in)
Depth at rim (including handle) - 138 mm (5.4 in)
Height - 122 mm (4.8 in)
Weight - 418 grams (14.7 oz)

Price:$40.00 (Not for sale, pieces being held for demo purposes)